FCNS03 Fe Cu Ni Sn Pre Alloyed Powder for Ceramic Diamond Blade
FCNS03 Fe Cu Ni Sn Pre Alloyed Powder for Ceramic Diamond Blade
1. Waa maxay budada hore loo daweeyay
Budada daawaynta hore loo sameeyay way adagtahay, way yartahay cufnaanta sidaa awgeed waxay u baahan yihiin culaysyo cadaadis sare leh si ay u soo saaraan cufnaanta sare.Si kastaba ha ahaatee, waxay awood u leeyihiin inay soo saaraan qalab sinteed xoog sare leh.Alloying-ka ka hor waxa kale oo la isticmaalaa marka wax-soo-saarka maaddooyinka isku midka ah ee budada curiyaha ah ay u baahan yihiin heerkul aad u sarreeya iyo wakhtiyo dheeraan ah.Tusaalooyinka ugu fiican waa birta aan-ka-soo-baxa lahayn, kuwaas oo chromium iyo nikkel ka kooban ay tahay in la sii daayo si loogu oggolaado wax soo saarka dhaqaale ee birta budada ah.
2. HalbeegyadaFCNS03
Cunsurka ugu muhiimsan | Fe, Ku, Ni, Sn | |
Cufnaanta Aragtida | 7.98g/cm³ | |
Heerkulka Sintering | 830℃ | |
Xoog Laabashada | 1150Mpa | |
Adag | 104-108HRB |
3. FCNS03 Dabeecad
- Qaab dhismeedka Sintered waa mid isku mid ah oo is haysta.bakhtigu wuxuu leeyahay xakameyn wanaagsan oo dheeman ah, caabbinta xirashada weyn iyo fiiqan.
- Budada waxaa lagu dabaqaa dhex dhexaad ama tayo sare leh daab dheeman granite ah, garbaha jarista dhoobada.
4. Tilmaamaha samaynta daab goynta dhoobada.
- Boqolkiiba Birta:
- (30-50)% FCNS03
- + (25-35)% Cu
- + (5-8)% Sn
- + (2-4)% Ni
- + Fe for Blance
B. Cabbirka Dheeman Grit iyo Boqolkiiba:
- 50/60 @ 30%
- 60/70 @ 40%
- 70/80 @ 30%
- Xoog-saarista: (9-12)%
C. Heerkulka Heerkulka: 840-860 ℃